ID
|
6
|
Symbol
|
CoPt
|
Image
|
|
Name
|
Cobalt Platinum
|
Categories
|
Iron group metals and alloys
|
Density (g/cm<sup>3</sup>)
|
16.04
|
Structure
|
L<sub>10</sub> tetragonal
|
Order
|
Ferromagnet
|
Curie temperature (K)
|
840
|
Cubic lattice parameter (p<sub>m</sub>) (a<sub>0</sub>)
|
|
Magnet ideality factor (p<sub>m</sub>) (a)
|
377
|
Resistivity (μΩ·m) (ρ)
|
|
Magnetic moment per unit mass (A m<sup>2</sup> kg<sup>-1</sup>) (σ)
|
50
|
Exchange stiffness (pJ m<sup>-1</sup>) (A)
|
10
|
Magnetic hardness parameter (κ)
|
2.47
|
Spontaneous magnetization (MA m<sup>-1</sup>) M<sub>s</sub>)
|
0.80
|
Spontaneous linear magnetostriction (λ<sub>s</sub>)
|
|
Anisotropy constants (KJ m<sup>-3</sup>) (K1)
|
4900
|
Magnetic polarization (T) (J<sub>s</sub>)
|
1.01
|
Image Source
|
https://www.technology.matthey.com/article/37/3/130-135/
|